Heat deflection temperature, 1.80 MPa: 213 °C

Quick Comparison

Polyketone (PK)

TECACOMP PK TRM XS black 4179

Geliefert von:

Ensinger GmbH

Polybutylenterephthalat (PBT)

LNP™ THERMOTUF™ Compound WF009NA

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

Arnite® TV4 270

Geliefert von:

DSM Engineering Materials

Polyamide 6 (PA6)

Zytel® 73G45L NC010

Polyethersulfon (PES)

LNP™ THERMOCOMP™ Compound JF006EXZ

Geliefert von:

Sabic

Polyetherimid (PEI)

LNP™ THERMOCOMP™ Compound EX11414

Geliefert von:

Sabic

Polyetherimid (PEI)

LNP™ THERMOCOMP™ Compound EC002XXQ

Geliefert von:

Sabic

Polyetherimid (PEI)

LNP™ THERMOCOMP™ Compound 9X99089

Geliefert von:

Sabic

Polyamide 6 (PA6)

LNP™ THERMOCOMP™ Compound PX87791

Geliefert von:

Sabic

Polyetherimid (PEI)

LNP™ LUBRICOMP™ Compound EX10405H

Geliefert von:

Sabic

Polyamide 610 (PA610)

LNP™ THERMOCOMP™ Compound QC006 - Europe

Geliefert von:

Sabic