Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.4 g/cm³ Show Supplier Material materials with Dichte of 1.4 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 234 MPa Show Supplier Material materials with Biegefestigkeit of 234 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 12.4 GPa Show Supplier Material materials with Biegemodul of 12.4 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 1.6 % Show Supplier Material materials with Dehnung of 1.6 % | ASTM D 638 | break |
Elastizitätsmodul | 23.0 °C | 14.2 GPa Show Supplier Material materials with Elastizitätsmodul of 14.2 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 58 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 58 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 552 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 552 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 58 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 58 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 154 MPa Show Supplier Material materials with Zugfestigkeit of 154 MPa | ASTM D 638 | break |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 235 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 235 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 235 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 235 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282587- - <br> UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=103093600- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device | |
Availability | Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |