Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.83 g/cm³ Show Supplier Material materials with Dichte of 1.83 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 140 MPa Show Supplier Material materials with Biegefestigkeit of 140 MPa | ISO 178 | break, 2 mm/min |
Biegemodul | 23.0 °C | 7.4 GPa Show Supplier Material materials with Biegemodul of 7.4 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 8 GPa Show Supplier Material materials with Elastizitätsmodul of 8 GPa | ISO 527 | 1 mm/min |
Hardness, Ball Indentation | 23.0 °C | 145 MPa Show Supplier Material materials with Hardness, Ball Indentation of 145 MPa | ISO 2039-1 | H358/30 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 35 kJ/m² | ISO 179/1eU | Unnotch Edgew 80*10*4 sp=62mm, -30°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 33 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 33 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Taber Abrasion | 23.0 °C | 76 mg/1000cy Show Supplier Material materials with Taber Abrasion of 76 mg/1000cy | SABIC method | CS-17, 1 kg |
Zugfestigkeit | 23.0 °C | 100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Heat deflection temperature, 0.45 MPa | 220 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 220 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 180 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 180 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Vicat-Erweichungstemperatur | 220 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 220 °C | ISO 306 | Rate A/50 | |||
Wärmeformbeständigkeitstemperatur | 180 - 220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 180 - 220 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.33 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.33 W/(m·K) | ISO 8302 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 8E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Entflammbarkeit | Glow Wire Flammability Index 750°C, passes at: 3.2mm IEC 60695-2-12 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 3.6 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3.6 [-] | IEC 60250 | 50/60 Hz |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 3.5 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.01 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 1E-3 [-] | IEC 60250 | 50/60 Hz |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 11 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 11 cm³/10min | ISO 1133 | MVR at 265°C/1.2 kg | |
Schrumpfung | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |