Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.41 - 0.5 [-] Show Supplier Material materials with Coefficient of friction of 0.41 - 0.5 [-] | ||
Coefficient of friction, kinetic | 0.41 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.41 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.5 [-] Show Supplier Material materials with Coefficient of friction, static of 0.5 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.7 g/cm³ Show Supplier Material materials with Dichte of 1.7 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 234 MPa Show Supplier Material materials with Biegefestigkeit of 234 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 14.2 GPa Show Supplier Material materials with Biegemodul of 14.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 1.6 % Show Supplier Material materials with Dehnung of 1.6 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 14.1 GPa Show Supplier Material materials with Elastizitätsmodul of 14.1 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 96 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 96 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 534 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 534 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 96 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 96 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 140 MPa Show Supplier Material materials with Zugfestigkeit of 140 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 264 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 264 °C | ASTM D 648 | 3.2mm, unannealed | |
Wärmeformbeständigkeitstemperatur | 264 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 264 °C | ||
Entflammbarkeit | UL Compliant, 94V-0 Flame Class Rating: 0.45mm UL 94 by SABIC-IP |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |