Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 4.54 g/cm³ Show Supplier Material materials with Dichte of 4.54 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % |
Elastizitätsmodul | 23.0 °C | 116 GPa Show Supplier Material materials with Elastizitätsmodul of 116 GPa |
Härte, Brinell | 23.0 °C | 120 [-] Show Supplier Material materials with Härte, Brinell of 120 [-] |
Streckgrenze | 23.0 °C | 170 - 310 MPa Show Supplier Material materials with Streckgrenze of 170 - 310 MPa |
Zugfestigkeit | 23.0 °C | 240 MPa Show Supplier Material materials with Zugfestigkeit of 240 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.6E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.6E-6 1/K |
Schmelzpunkt | 1668 °C Show Supplier Material materials with Schmelzpunkt of 1668 °C | |
Wärmeleitfähigkeit | 23.0 °C | 21.9 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 21.9 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Welding wires, MMO Wire Anodes, Racks, Glass frames | |
Chemical composition | Purity of 99.99% | |
Processing history | It is drawn from forged rods. SAM operates a strict quality control process using ASTM grades of titanium to ensure no contamination. |