Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10.28 g/cm³ Show Supplier Material materials with Dichte of 10.28 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 329 GPa Show Supplier Material materials with Elastizitätsmodul of 329 GPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.8E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.8E-6 1/K |
Schmelzpunkt | 2623 °C Show Supplier Material materials with Schmelzpunkt of 2623 °C | |
Wärmeleitfähigkeit | 23.0 °C | 138 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 138 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Used for processing fabricated metal products and machine parts such as wire, sheets, sintered alloys, and electronic components. Used for alloying, brake pads, ceramic metallization, diamond tooling, infiltration, and metal injection molding. Used as a chemical catalyst, detonation initiator, metal matrix composite, and sputtering target. | |
Chemical composition | Purity of ≥99.95% | |
Processing history | Molybdenum powder is produced by hydrogen reduction of molybdenum trioxide and ammonium molybdates. |