Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 11.6 g/cm³ Show Supplier Material materials with Dichte of 11.6 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % |
Härte, Shore A | 23.0 °C | 95 [-] Show Supplier Material materials with Härte, Shore A of 95 [-] |
Reißfestigkeit | 23.0 °C | 18 kN/m Show Supplier Material materials with Reißfestigkeit of 18 kN/m |
Zugfestigkeit | 23.0 °C | 5.9 MPa Show Supplier Material materials with Zugfestigkeit of 5.9 MPa |
Technological properties
Property | ||
---|---|---|
Application areas | Radiation shielding and radiation-protective equipment, X-ray inspection device for industrial and medical use, ϒ-ray shielding material and substitute for lead fiber mat in nuclear reactor piping systems. |