Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 462 MPa Show Supplier Material materials with Biegefestigkeit of 462 MPa | For ceramic structural parts |
Elastizitätsmodul | 23.0 °C | 393 GPa Show Supplier Material materials with Elastizitätsmodul of 393 GPa | For ceramic structural parts |
Plane-Strain Fracture Toughnes | 23.0 °C | 4 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 MPa·√m | For ceramic structural parts |
Poissonzahl | 23.0 °C | 0.2 [-] Show Supplier Material materials with Poissonzahl of 0.2 [-] | For ceramic structural parts |
Zugfestigkeit | 23.0 °C | 307 MPa Show Supplier Material materials with Zugfestigkeit of 307 MPa | For ceramic structural parts |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.3E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.3E-6 1/K | For ceramic structural parts |
Max. Betriebstemperatur | 1000 °C Show Supplier Material materials with Max. Betriebstemperatur of 1000 °C | For ceramic structural parts | |
Spezifische Wärmekapazität | 23.0 °C | 880 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 880 J/(kg·K) | For ceramic structural parts |
Wärmeleitfähigkeit | 23.0 °C | 125 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 125 W/(m·K) | For ceramic structural parts |
Technological properties
Property | ||
---|---|---|
Application areas | Used in semiconductor and coating industries, As a bearing material for magnetic drive pumps for many years. It is useful in a variety of applications including spray nozzles, shot blast nozzles and cyclone components | |
Chemical composition | SiC, ZrO2, Si3N4 | |
Processing history | Reaction Bonded |