Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Polymer Silicon Carbide Composite SICAPRINT™ P100
Pragmatic solution for functional parts that are exposed to abrasive and corrosive fluids and constant temperatures up to 200 °C. The simple refinement process allows for economical solutions.
Depending on the technical requirements a variety of resins is being held on demand to realize the desired result.
The advantages of SICAPRINT™ are:
Diese Materialdaten wurden von SGL Carbon zur Verfügung gestellt
See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
All categories
Allgemein
Property | Value |
---|---|
Dichte | 2 g/cm³ Show Supplier Material materials with Dichte of 2 g/cm³ |
Mechanisch
Property | Value |
---|---|
Biegefestigkeit | 55 MPa Show Supplier Material materials with Biegefestigkeit of 55 MPa |
Druckfestigkeit | 130 MPa Show Supplier Material materials with Druckfestigkeit of 130 MPa |
Elastizitätsmodul | 19 GPa Show Supplier Material materials with Elastizitätsmodul of 19 GPa |
Härte, Shore D | 90.0 [-] Show Supplier Material materials with Härte, Shore D of 90.0 [-] |
Thermisch
Property | Value |
---|---|
Wärmeleitfähigkeit | 2.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 2.6 W/(m·K) |
Technological properties
Property |
---|
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.