Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Want to keep this datasheet? Save it now in your required format
Description
SIGRATHERM® ePCM Composite Materials guarantee high storage density and fast charge/discharge cycles.
Phase Change Materials (PCM) are materials whose latent heat produced mainly at the solid-liquid phase transition point (heat of fusion), is used in technical applications. Water/ice is the best-known example of a PCM. Salt hydrates as well as paraffins are among the PCMs widely used for other temperature requirements. Pure PCM show high storage density, long charging and discharging cycles and low thermal conductivity.
SIGRATHERM ePCM is a graphite/PCM compound material made from expanded graphite with encapsulated PCM material. It is supplied in plates and sheets.
Diese Materialdaten wurden von SGL Carbon zur Verfügung gestellt
Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert. Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.