SIGRATHERM® Water Based Graphite Dispersions Grade A
Description
Dispersions based on expanded graphite powders and graphite nanoplates.
Expanded graphite nanoplates consist of small, 1-15 nanometer thick, single or multilayer graphite layers, with diameters up to 100 micrometers. They constitute a new class of graphite nanoparticles with multifunctional properties. In order to obtain a graphite dispersion, small graphite particles and nanoplates produced by secondary treatment of our expanded graphite are mixed with a dispersant in water. Depending on the application, the viscosity of the dispersion can be adjusted by means of different concentrations of solids. The maximum dispersible solid content is 5.5% by weight.
Key characteristics of our graphite nanoplates are:
- Excellent layer formation on a variety of substrates, e.g. copper foil or PET film
- The high aspect ratio of the graphite nanoplates allows high electrical and thermal conductivity
- Freestanding graphite foils with a thickness between 5 and 15 μm can be produced
Diese Materialdaten wurden von SGL Carbon zur Verfügung gestellt
Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.