Allgemein
Property | Value | Comment |
---|---|---|
Korngröße | 15.0 μm Show Supplier Material materials with Korngröße of 15.0 μm | |
Permeabilitätskoeffizient | 0.25 cm²/s Show Supplier Material materials with Permeabilitätskoeffizient of 0.25 cm²/s | |
Porosität | 15.0 % Show Supplier Material materials with Porosität of 15.0 % | open porosity |
Schüttdichte | 1.72 g/cm³ Show Supplier Material materials with Schüttdichte of 1.72 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 45 MPa Show Supplier Material materials with Biegefestigkeit of 45 MPa | |
Druckfestigkeit | 90 MPa Show Supplier Material materials with Druckfestigkeit of 90 MPa | |
Elastizitätsmodul | 11 GPa Show Supplier Material materials with Elastizitätsmodul of 11 GPa | Dynamic Modulus |
Hardness, Rockwell | 80.0 [-] Show Supplier Material materials with Hardness, Rockwell of 80.0 [-] | 10/100 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 0.0005 % Show Supplier Material materials with Aschegehalt of 0.0005 % | depending on the code, it can also be less than 5 ppm | |
0.003 % Show Supplier Material materials with Aschegehalt of 0.003 % | depending on the code, it can also be less than 5 ppm | ||
Koeffizient der thermischen Ausdehnung | 3.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.2e-06 1/K | @20-200°C | |
Wärmeleitfähigkeit | 20 °C | 105 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 105 W/(m·K) |
Elektrisch
Property | Value |
---|---|
spezifischer Widerstand | 1.2e-05 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.2e-05 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 1e-06 - 5e-06 % Show Supplier Material materials with Aluminium of 1e-06 - 5e-06 % | depending on the code, it can also be less |
Bor | 2e-06 - 1e-05 % Show Supplier Material materials with Bor of 2e-06 - 1e-05 % | depending on the code, it can also be less |
Chrom | 1e-06 - 2e-06 % Show Supplier Material materials with Chrom of 1e-06 - 2e-06 % | depending on the code, it can also be less |
Eisen | 2e-06 - 5e-05 % Show Supplier Material materials with Eisen of 2e-06 - 5e-05 % | depending on the code |
Kalzium | 1e-06 - 2e-05 % Show Supplier Material materials with Kalzium of 1e-06 - 2e-05 % | depending on the code |
Kobalt | 1e-06 - 2e-06 % Show Supplier Material materials with Kobalt of 1e-06 - 2e-06 % | depending on the code, it can also be less |
Kupfer | 1e-06 - 2e-06 % Show Supplier Material materials with Kupfer of 1e-06 - 2e-06 % | depending on the code, it can also be less |
Magnesium | 1e-06 - 1e-05 % Show Supplier Material materials with Magnesium of 1e-06 - 1e-05 % | depending on the code |
Mangan | 1e-06 % Show Supplier Material materials with Mangan of 1e-06 % | max. |
Nickel | 1e-06 - 0.0001 % Show Supplier Material materials with Nickel of 1e-06 - 0.0001 % | depending on the code, it can also be less |
Phosphor | 2e-06 - 1e-05 % Show Supplier Material materials with Phosphor of 2e-06 - 1e-05 % | depending on the code, it can also be less |
Silizium | 0.0001 - 0.0002 % Show Supplier Material materials with Silizium of 0.0001 - 0.0002 % | depending on the code, it can also be less |
Titan | 1e-06 - 2e-05 % Show Supplier Material materials with Titan of 1e-06 - 2e-05 % | depending on the code |
Vanadium | 1e-06 - 5e-05 % Show Supplier Material materials with Vanadium of 1e-06 - 5e-05 % | depending on the code |
Technological properties
Property | ||
---|---|---|
Processing methods | Isostatically pressed |