Allgemein
Property | Value | Comment |
---|---|---|
Partikelgröße D50 | 51.0 μm Show Supplier Material materials with Partikelgröße D50 of 51.0 μm | |
Spezifische Oberfläche | 1.25 m²/g Show Supplier Material materials with Spezifische Oberfläche of 1.25 m²/g | BET; DIN ISO 9277 |
Tap density | 0.18 g/cm³ Show Supplier Material materials with Tap density of 0.18 g/cm³ | ASTM D3800 |
True particle density | 0.45 g/cm³ Show Supplier Material materials with True particle density of 0.45 g/cm³ | DIN 51913 |
Water content | 0.1 % Show Supplier Material materials with Water content of 0.1 % | ASTM C562 |
Abmessung
Property | Temperature | Value |
---|---|---|
Dimensions | Particle size D50 = 51 μm (ISO 13320) °C | Particle size < 50 mesh/300 µm: 98% (ASTM E11) |
Mechanisch
Property | Value | Comment |
---|---|---|
Druckfestigkeit | 2.0 - 4.2 MPa Show Supplier Material materials with Druckfestigkeit of 2.0 - 4.2 MPa | ASTM D3102-78, minimum value for 90% and maximum value for 80% survival |
Thermisch
Property | Value | Comment |
---|---|---|
Aschegehalt | 0.2 % Show Supplier Material materials with Aschegehalt of 0.2 % | ASTM C561 |