Allgemein
Property | Value |
---|---|
Dichte | 1.4 g/cm³ Show Supplier Material materials with Dichte of 1.4 g/cm³ |
Mechanisch
Property | Value |
---|---|
Biegefestigkeit | 400 MPa Show Supplier Material materials with Biegefestigkeit of 400 MPa |
Biegemodul | 50 GPa Show Supplier Material materials with Biegemodul of 50 GPa |
Elastizitätsmodul | 44 GPa Show Supplier Material materials with Elastizitätsmodul of 44 GPa |
Failure Strain | 1.2 % Show Supplier Material materials with Failure Strain of 1.2 % |
Zugfestigkeit | 570.0 MPa Show Supplier Material materials with Zugfestigkeit of 570.0 MPa |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | Components and assemblies based on plate material (liquid distributors, collectors, support grids, retainers) |