Allgemein
Property | Value |
---|---|
Dichte | 1.5 g/cm³ Show Supplier Material materials with Dichte of 1.5 g/cm³ |
Mechanisch
Property | Value |
---|---|
Biegefestigkeit | 340 MPa Show Supplier Material materials with Biegefestigkeit of 340 MPa |
Biegemodul | 75 GPa Show Supplier Material materials with Biegemodul of 75 GPa |
Elastizitätsmodul | 65 GPa Show Supplier Material materials with Elastizitätsmodul of 65 GPa |
Failure Strain | 0.4 % Show Supplier Material materials with Failure Strain of 0.4 % |
Zugfestigkeit | 270.0 MPa Show Supplier Material materials with Zugfestigkeit of 270.0 MPa |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | Components and assemblies based on plate material (liquid distributors, collectors, support grids, retainers) |