Allgemein
Property | Value |
---|---|
Dichte | 1.5 g/cm³ Show Supplier Material materials with Dichte of 1.5 g/cm³ |
Mechanisch
Property | Value |
---|---|
Biegefestigkeit | 100 MPa Show Supplier Material materials with Biegefestigkeit of 100 MPa |
Biegemodul | 28 GPa Show Supplier Material materials with Biegemodul of 28 GPa |
Elastizitätsmodul | 35 GPa Show Supplier Material materials with Elastizitätsmodul of 35 GPa |
Interlaminare Scherfestigkeit | 11.0 MPa Show Supplier Material materials with Interlaminare Scherfestigkeit of 11.0 MPa |
Zugfestigkeit | 65.0 MPa Show Supplier Material materials with Zugfestigkeit of 65.0 MPa |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | Connection elements (nuts, bolds, screws, rods) |