Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 38 % Show Supplier Material materials with Dehnung of 38 % |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa |
Streckgrenze | 23.0 °C | 210 MPa Show Supplier Material materials with Streckgrenze of 210 MPa |
Zugfestigkeit | 23.0 °C | 270 - 370 MPa Show Supplier Material materials with Zugfestigkeit of 270 - 370 MPa |
Chemical properties
Property | Value |
---|---|
Eisen | Balance |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % |
Mangan | 0.4 % Show Supplier Material materials with Mangan of 0.4 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |