Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 33 % Show Supplier Material materials with Dehnung of 33 % |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa |
Streckgrenze | 23.0 °C | 185 - 195 MPa Show Supplier Material materials with Streckgrenze of 185 - 195 MPa |
Zugfestigkeit | 23.0 °C | 315 - 430 MPa Show Supplier Material materials with Zugfestigkeit of 315 - 430 MPa |