Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 17 % Show Supplier Material materials with Dehnung of 17 % |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa |
Streckgrenze | 23.0 °C | 235 - 245 MPa Show Supplier Material materials with Streckgrenze of 235 - 245 MPa |
Zugfestigkeit | 23.0 °C | 400 - 510 MPa Show Supplier Material materials with Zugfestigkeit of 400 - 510 MPa |
Chemical properties
Property | Value |
---|---|
Eisen | Balance |
Kohlenstoff | 0.21 % Show Supplier Material materials with Kohlenstoff of 0.21 % |
Mangan | 1.4 % Show Supplier Material materials with Mangan of 1.4 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |