Property | Value | Comment |
---|---|---|
Dichte | 1.29 g/cm³ Show Supplier Material materials with Dichte of 1.29 g/cm³ | ASTM D792 |
Abmessung
Property | Value |
---|---|
Durchmesser | 1.75 mm Show Supplier Material materials with Durchmesser of 1.75 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 26.0 % Show Supplier Material materials with Dehnung of 26.0 % | ASTM D638 |
Elastizitätsmodul | 3.12 GPa Show Supplier Material materials with Elastizitätsmodul of 3.12 GPa | ASTM D638 |
Elongation at yield | 4.8 % Show Supplier Material materials with Elongation at yield of 4.8 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 81.0 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 81.0 J/m | ASTM D256 |
Streckgrenze | 85.0 MPa Show Supplier Material materials with Streckgrenze of 85.0 MPa | ASTM D638 |
Zugfestigkeit | 48.0 MPa Show Supplier Material materials with Zugfestigkeit of 48.0 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 343.0 °C Show Supplier Material materials with Schmelzpunkt of 343.0 °C | ASTM D3418 |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace Applications, Automotive Applications, Oil/Gas Applications | |
Certifications | Substances used to manufacture the polymer grade used for this filament meets the requirements of Commission Regulation (EU) N°10/2011, which implements the framework regulation EU 1935/2004 as related to plastic materials and articles intended to come into contact with food and its subsequent amendments as well as the GMP requirements for EU 2023/2006. Please feel free to contact the supplier for RoHS Compliance. | |
Color | Natural | |
Features | ||
Other | Test specimen parameters:
Note: Typical properties: these are not to be construed as specifications | |
Processing methods | Fused Filament Fabrication (FFF) Printing conditions for above data table: |