Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.72 g/cm³ Show Supplier Material materials with Dichte of 1.72 g/cm³ | ASTM D792, ¹ |
Abmessung
Property | Value |
---|---|
Durchmesser | 2.85 mm Show Supplier Material materials with Durchmesser of 2.85 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 50.0 - 250.0 % Show Supplier Material materials with Dehnung of 50.0 - 250.0 % | ASTM D638, ² |
Elastizitätsmodul | 0.8 GPa Show Supplier Material materials with Elastizitätsmodul of 0.8 GPa | ASTM D638, ² |
Elongation at yield | 10.0 % Show Supplier Material materials with Elongation at yield of 10.0 % | ASTM D638, ² |
Schlagfestigkeit, Charpy gekerbt | 6.0 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6.0 kJ/m² | |
Streckgrenze | 30.0 MPa Show Supplier Material materials with Streckgrenze of 30.0 MPa | ASTM D638, ² |
Zugfestigkeit | 25.0 MPa Show Supplier Material materials with Zugfestigkeit of 25.0 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 148.0 °C Show Supplier Material materials with Schmelzpunkt of 148.0 °C | ASTM D3418 |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Manufacturing (3D Printing), Industrial applications, Oil/Gas applications, Plumbing applications | |
Certifications | Substances used to manufacture the polymer grade used for this filament meets the requirements of Commission Regulation (EU) N°10/2011, which implements the framework regulation EU 1935/2004 as related to plastic materials and articles intended to come into contact with food and its subsequent amendments as well as the GMP requirements for EU 2023/2006. Please feel free to contact the supplier for RoHS Compliance. | |
Color | White | |
Features | ||
Other | Test specimen parameters:
Note: Typical properties: these are not to be construed as specifications ¹On 3D printed specimens ²On 3D printed specimens, x-direction | |
Processing methods | Fused Filament Fabrication (FFF) Printing conditions for above data table: |