Abmessung
Property | Value |
---|---|
Durchmesser | 25.4 - 355.6 mm Show Supplier Material materials with Durchmesser of 25.4 - 355.6 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 8 % Show Supplier Material materials with Dehnung of 8 % |
Härte, Brinell | 23.0 °C | 388 [-] Show Supplier Material materials with Härte, Brinell of 388 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 1170 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 1170 MPa |
Zugfestigkeit | 23.0 °C | 1310 MPa Show Supplier Material materials with Zugfestigkeit of 1310 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Andere | 0.15 - 0.45 % Show Supplier Material materials with Andere of 0.15 - 0.45 % | Nb+Ta | |
Chrom | 15 - 17.5 % Show Supplier Material materials with Chrom of 15 - 17.5 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.07 % Show Supplier Material materials with Kohlenstoff of 0.07 % | ||
Kupfer | 3 - 5 % Show Supplier Material materials with Kupfer of 3 - 5 % | ||
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | ||
Nickel | 3 - 5 % Show Supplier Material materials with Nickel of 3 - 5 % | ||
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | ||
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | ||
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | chemical, petrochemical, paper and general metalworking industries | |
Heat Treatment | Solution annealing at 1000 to 1050°C, hardened at 480°C | |
Welding | Good, Pre-heating and post-heating practices used for standard hardenable stainless grades are not required. Min. RREN: 17 |