Abmessung
Property | Value |
---|---|
Breite | 2000 mm Show Supplier Material materials with Breite of 2000 mm |
Dicke | 10 - 50 mm Show Supplier Material materials with Dicke of 10 - 50 mm |
Länge | 4000 - 6000 mm Show Supplier Material materials with Länge of 4000 - 6000 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -40.0 °C | 50 J Show Supplier Material materials with Charpy impact energy, V-notch of 50 J | |
Dehnung | 23.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % | |
Streckgrenze Rp 0,2 | 23.0 °C | 450 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 450 MPa | T≥10MM |
Zugfestigkeit | 23.0 °C | 650 MPa Show Supplier Material materials with Zugfestigkeit of 650 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 21 - 22 % Show Supplier Material materials with Chrom of 21 - 22 % |
Eisen | Balance |
Kohlenstoff | 0.04 % Show Supplier Material materials with Kohlenstoff of 0.04 % |
Kupfer | 0.1 - 0.8 % Show Supplier Material materials with Kupfer of 0.1 - 0.8 % |
Mangan | 4 - 6 % Show Supplier Material materials with Mangan of 4 - 6 % |
Molybdän | 0.1 - 0.8 % Show Supplier Material materials with Molybdän of 0.1 - 0.8 % |
Nickel | 1.35 - 1.9 % Show Supplier Material materials with Nickel of 1.35 - 1.9 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.2 - 0.25 % Show Supplier Material materials with Stickstoff of 0.2 - 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Ideal for tank production where corrosion strength is sufficient | |
Corrosion properties | High resistance to stress corrosion cracking, Good resistance to general corrosion.PREN=26 | |
Heat Treatment | Solution annealing at 1020 – 1100°C followed by water quenching. | |
Welding | Very good |