Abmessung
Property | Value |
---|---|
Durchmesser | 3 - 650 mm Show Supplier Material materials with Durchmesser of 3 - 650 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -195.0 °C | 60 J Show Supplier Material materials with Charpy impact energy, V-notch of 60 J |
Dehnung | 23.0 °C | 30 - 40 % Show Supplier Material materials with Dehnung of 30 - 40 % |
Härte, Brinell | 23.0 °C | 215 [-] Show Supplier Material materials with Härte, Brinell of 215 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 205 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 205 MPa |
Zugfestigkeit | 23.0 °C | 515 - 690 MPa Show Supplier Material materials with Zugfestigkeit of 515 - 690 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 16 - 18 % Show Supplier Material materials with Chrom of 16 - 18 % |
Eisen | Balance |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Molybdän | 2 - 3 % Show Supplier Material materials with Molybdän of 2 - 3 % |
Nickel | 10 - 14 % Show Supplier Material materials with Nickel of 10 - 14 % |
Phosphor | 0.45 % Show Supplier Material materials with Phosphor of 0.45 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 0.75 % Show Supplier Material materials with Silizium of 0.75 % |
Stickstoff | 0.01 % Show Supplier Material materials with Stickstoff of 0.01 % |
Technological properties
Property | ||
---|---|---|
Application areas | The austenitic stainless steel AISI 316L shows good acid resistance. Material AISI 316L is used in the chemical industry, apparatus engineering, sewage plants and piping industry. | |
Heat Treatment | Solution annealed and quenched in air or water. | |
Welding | Very good |