Abmessung
Property | Value |
---|---|
Durchmesser | 12.7 - 304.8 mm Show Supplier Material materials with Durchmesser of 12.7 - 304.8 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -101.0 °C | 27 J Show Supplier Material materials with Charpy impact energy, V-notch of 27 J |
Dehnung | 23.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % |
Härte, Brinell | 23.0 °C | 248 - 363 [-] Show Supplier Material materials with Härte, Brinell of 248 - 363 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 725 - 1000 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 725 - 1000 MPa |
Zugfestigkeit | 23.0 °C | 895 - 1250 MPa Show Supplier Material materials with Zugfestigkeit of 895 - 1250 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.2 - 0.8 % Show Supplier Material materials with Aluminium of 0.2 - 0.8 % | |
Andere | 4.75 - 5.5 % Show Supplier Material materials with Andere of 4.75 - 5.5 % | Nb+Ta |
Chrom | 17 - 21 % Show Supplier Material materials with Chrom of 17 - 21 % | |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | |
Kupfer | 0.3 % Show Supplier Material materials with Kupfer of 0.3 % | |
Mangan | 0.35 % Show Supplier Material materials with Mangan of 0.35 % | |
Molybdän | 2.8 - 3.3 % Show Supplier Material materials with Molybdän of 2.8 - 3.3 % | |
Nickel | 50 - 55 % Show Supplier Material materials with Nickel of 50 - 55 % | |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | |
Silizium | 0.35 % Show Supplier Material materials with Silizium of 0.35 % | |
Titan | 0.65 - 1.05 % Show Supplier Material materials with Titan of 0.65 - 1.05 % |
Technological properties
Property | ||
---|---|---|
Application areas | Used in pumps, tooling, gas turbines rocket motors and nuclear reactors. | |
Heat Treatment | Solution annealed at 1000 – 1052°C. Age hardening at 774 – 802°C. | |
Welding | Very good |