Abmessung
Property | Value |
---|---|
Durchmesser | 25.4 - 230 mm Show Supplier Material materials with Durchmesser of 25.4 - 230 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -196.0 °C | 357 J Show Supplier Material materials with Charpy impact energy, V-notch of 357 J |
Dehnung | 23.0 °C | 40 % Show Supplier Material materials with Dehnung of 40 % |
Härte, Brinell | 23.0 °C | 240 [-] Show Supplier Material materials with Härte, Brinell of 240 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 300 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 300 MPa |
Zugfestigkeit | 23.0 °C | 700 MPa Show Supplier Material materials with Zugfestigkeit of 700 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 14.5 - 16.5 % Show Supplier Material materials with Chrom of 14.5 - 16.5 % |
Eisen | 4 - 7 % Show Supplier Material materials with Eisen of 4 - 7 % |
Kobalt | 2.5 % Show Supplier Material materials with Kobalt of 2.5 % |
Kohlenstoff | 0.01 % Show Supplier Material materials with Kohlenstoff of 0.01 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Molybdän | 15 - 17 % Show Supplier Material materials with Molybdän of 15 - 17 % |
Nickel | Balance |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 0.08 % Show Supplier Material materials with Silizium of 0.08 % |
Vanadium | 0.35 % Show Supplier Material materials with Vanadium of 0.35 % |
Wolfram | 3 - 4.5 % Show Supplier Material materials with Wolfram of 3 - 4.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Usually used in chemical processing, pollution control, pulp and paper industry, waste treatment, dampers, scrubbers and heat exchangers. | |
Corrosion properties | This alloy has excellent resistance to pitting and stress corrosion cracking and oxidizing atmospheres up to 1040°C. Alloy C-276 exhibits excellent resistance in a wide variety of chemical process environments including those with ferric and cupric chlorides, hot contaminated organic and inorganic media, chlorine, formic and acetic acids, seawater, brine and hypochlorite and chlorine dioxide solutions. | |
Heat Treatment | Solution annealed at 1100 to 1160°C | |
Welding | Good |