Abmessung
Property | Value |
---|---|
Durchmesser | 10 - 300 mm Show Supplier Material materials with Durchmesser of 10 - 300 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 20 % Show Supplier Material materials with Dehnung of 20 % |
Härte, Rockwell B | 23.0 °C | 160 [-] Show Supplier Material materials with Härte, Rockwell B of 160 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 276 - 448 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 276 - 448 MPa |
Zugfestigkeit | 23.0 °C | 345 MPa Show Supplier Material materials with Zugfestigkeit of 345 MPa |
Chemical properties
Property | Value |
---|---|
Eisen | 0.3 % Show Supplier Material materials with Eisen of 0.3 % |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % |
Sauerstoff | 0.25 % Show Supplier Material materials with Sauerstoff of 0.25 % |
Stickstoff | 0.03 % Show Supplier Material materials with Stickstoff of 0.03 % |
Titan | Balance |
Wasserstoff | 0.02 % Show Supplier Material materials with Wasserstoff of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | Grade 2 titanium is also used to manufacture heat exchangers and cryogenic vessels. In seawater, Grade 2 is fully resistant to corrosion at temperatures up to 300°C. | |
Corrosion properties | It is highly resistant to chemical environments including oxidizing media, alkaline media, organic acids and compounds, aqueous salt solutions and hot gases. Its corrosion resistance holds up in liquid metals, nitric acid, mildly reducing acids and wet chlorine or bromine gas. |