Abmessung
Property | Value |
---|---|
Durchmesser | 76.2 - 508 mm Show Supplier Material materials with Durchmesser of 76.2 - 508 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -32.0 °C | 42 J Show Supplier Material materials with Charpy impact energy, V-notch of 42 J |
Dehnung | 23.0 °C | 17 - 18 % Show Supplier Material materials with Dehnung of 17 - 18 % |
Härte, Rockwell C | 23.0 °C | 22 [-] Show Supplier Material materials with Härte, Rockwell C of 22 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 414 - 517 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 414 - 517 MPa |
Zugfestigkeit | 23.0 °C | 585 - 655 MPa Show Supplier Material materials with Zugfestigkeit of 585 - 655 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.8 - 1.1 % Show Supplier Material materials with Chrom of 0.8 - 1.1 % |
Eisen | Balance |
Kohlenstoff | 0.28 - 0.33 % Show Supplier Material materials with Kohlenstoff of 0.28 - 0.33 % |
Mangan | 0.4 - 0.6 % Show Supplier Material materials with Mangan of 0.4 - 0.6 % |
Molybdän | 0.15 - 0.25 % Show Supplier Material materials with Molybdän of 0.15 - 0.25 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % |
Silizium | 0.15 - 0.35 % Show Supplier Material materials with Silizium of 0.15 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | AISI 4130 is a low alloyed hardened and tempered steel used for Oil and gas drilling and production equipment – wellhead and Christmas tree equipment. | |
Heat Treatment | Hardened at 860°C followed by water quenching. Tempering at min. 650°C, cooled in air. | |
Welding | Good. |