Abmessung
Property | Value |
---|---|
Durchmesser | 76.2 - 254 mm Show Supplier Material materials with Durchmesser of 76.2 - 254 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -10.0 °C | 60 J Show Supplier Material materials with Charpy impact energy, V-notch of 60 J |
Dehnung | 23.0 °C | 20 % Show Supplier Material materials with Dehnung of 20 % |
Härte, Rockwell C | 23.0 °C | 27 [-] Show Supplier Material materials with Härte, Rockwell C of 27 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 655 - 724 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 655 - 724 MPa |
Zugfestigkeit | 23.0 °C | 724 MPa Show Supplier Material materials with Zugfestigkeit of 724 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 11.5 - 13.5 % Show Supplier Material materials with Chrom of 11.5 - 13.5 % |
Eisen | Balance |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Molybdän | 1.5 - 2.5 % Show Supplier Material materials with Molybdän of 1.5 - 2.5 % |
Nickel | 4.5 - 6 % Show Supplier Material materials with Nickel of 4.5 - 6 % |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % |
Schwefel | 5E-3 % Show Supplier Material materials with Schwefel of 5E-3 % |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % |
Titan | 0.01 - 0.5 % Show Supplier Material materials with Titan of 0.01 - 0.5 % |
Vanadium | 0.5 % Show Supplier Material materials with Vanadium of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Commonly used in the same area as AISI 4130, 4140 and 4145 but often in environment, which have a high content of sulfur. | |
Heat Treatment | Hardened and tempered | |
Welding | Moderate |