ASTM A1008 HSLA Grade 80 Brass-plated

Alternative und Handelsbezeichungen
Brass electroplated steel
Want to keep this datasheet? Save it now in your required format

Description

Tata Steel offers a range of cold-rolled steel strip products electroplated with brass. These products have excellent performance features and provide a cost-effective alternative to solid brass.


Our brass-plated steel products are used in numerous applications from sporting ammunition to household goods. Their consistent quality enables trouble-free processing.


Our cold-rolled steel strip is manufactured to consistently tight dimensional tolerances. Stringent process control ensures excellent adhesion of the pure brass layer during electroplating. The finished product has a brass layer that is uniform, clean and free of oxides. Our products are available in a choice of surface finish to suit your applications.


Tata Steel’s brass-plated steel strip products offer significant benefits for your processing operations. They have outstanding formability. Their deep-drawing properties enable reliable production of components in demanding shapes.


For added benefits, we can tailor our products to meet your exact processing and end-product requirements.


Main benefits of our brass-plated steel include:
  • end-products of consistent and reliable quality
  • improved end-product performance
  • trouble-free, repeatable processing
  • minimised waste
  • extended tool life
  • control of substrate and base metal properties

  • Related Standards

    Diese Materialdaten wurden von TATA Steel zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    Eigenschaften

    Chemical properties

    PropertyValueComment

    Andere

    0.005 %

    Show Supplier Material materials with Andere of 0.005 %

    min. Cb/Nb

    Chrom

    0.15 %

    Show Supplier Material materials with Chrom of 0.15 %

    max.

    Kohlenstoff

    0.15 %

    Show Supplier Material materials with Kohlenstoff of 0.15 %

    max.

    Kupfer

    0.2 %

    Show Supplier Material materials with Kupfer of 0.2 %

    max.

    Mangan

    1.65 %

    Show Supplier Material materials with Mangan of 1.65 %

    max.

    Molybdän

    0.16 %

    Show Supplier Material materials with Molybdän of 0.16 %

    max.

    Nickel

    0.2 %

    Show Supplier Material materials with Nickel of 0.2 %

    max.

    Phosphor

    0.02 %

    Show Supplier Material materials with Phosphor of 0.02 %

    max.

    Schwefel

    0.025 %

    Show Supplier Material materials with Schwefel of 0.025 %

    max.

    Titan

    0.005 %

    Show Supplier Material materials with Titan of 0.005 %

    min.

    Vanadium

    0.005 %

    Show Supplier Material materials with Vanadium of 0.005 %

    min.

    Technological properties

    Property
    Application areas

  • Sporting ammunition
  • Decorative household products
  • Automotive components

  • Other

    Surface roughness (Ra)
    KR 0 / Appliance FinishRa: ≤ 0.10 μm (exceptionally smooth mirror finish)
    KR 0.5Ra: ≤ 0.20 μm (very smooth bright finish)
    KR 4 / #2 FinishRa: 0.15 - 0.45 μm (smooth finish)
    KR 7 / #1 FinishRa: 0.6 - 1.8 μm (rough finish)
    KR 8 / #1 FinishRa: 1.0 - 2.5 μm (rough matt finish)


    Coil weight
    Strip thickness (mm / inch)max coil weight EU/US
    0.1 – 1.4 / 0.008” – 0.055”10kg/mm coil width (10 KIM) / 700 PIW


    Coil inner diameter (ID)
    mm / inch
    Coil outer diameter (OD)
    mm / inch
    400, 500 / 16”, 20”max. 1368 / 60”


    Coil edge finishes
    Natural edges (#2)strip edges have a mill edge (un-slit edges)
    Slit edges (#3)strip edges have been slit (reduces maximum width by a total of 10mm)
    Sheets cut to lengthstrip cut to a specific length (sheets)
    Straight wound coilsstandard
    Traverse wound coils (a spool)upon request – please consult us


    Delivery conditionThickness range (mm/inch)Plating thickness (μm/µ")Width range (mm/inch)
    LC, C290, C340, C390, C440, C490, C590, C690, 1T (full hard), 2T, 3T, 4T, 5T0.20 – 1.70 / 0.008 - 0.0701.5 - 5.0 / 60 - 2003 - 724 / 0.10 - 28.5

    Packaging size

    Skid Type (2 & 3 runners) Dimensions mm / inch
    Pallet (Eye to sky) Coil Pallet (Eye to the side) 2 - wayMinimum 660 x 660 / 26” x 26”
    4 - wayMaximum 1321 x 1321 / 52” x 52”
    Parameters selected to protect coils from overhanging skids
    Coil No Pallet (Eye to side)Shrouded / Stretch-wrapped


    Other packaging options are available – please consult us.

    Surface Finish

  • Natural brass finish
  • Roughness from smooth to heavy matt
  • Brushed finish

  • Surface protection

  • Our products can be delivered with adhesive protective foils on the surface including among others: oil-resistant PVC foil, PE foil or a special PE foil used for laser-cutting purposes.
  • In addition we apply oil according to your requirements.
  • Other surface protection options are available – please consult us.