Chemical properties
Property | Value | Comment |
---|---|---|
Andere | 0.005 % Show Supplier Material materials with Andere of 0.005 % | min. Cb/Nb |
Chrom | 0.15 % Show Supplier Material materials with Chrom of 0.15 % | max. |
Kohlenstoff | 0.15 % Show Supplier Material materials with Kohlenstoff of 0.15 % | max. |
Kupfer | 0.2 % Show Supplier Material materials with Kupfer of 0.2 % | max. |
Mangan | 1.65 % Show Supplier Material materials with Mangan of 1.65 % | max. |
Molybdän | 0.16 % Show Supplier Material materials with Molybdän of 0.16 % | max. |
Nickel | 0.2 % Show Supplier Material materials with Nickel of 0.2 % | max. |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | max. |
Titan | 0.005 % Show Supplier Material materials with Titan of 0.005 % | min. |
Vanadium | 0.005 % Show Supplier Material materials with Vanadium of 0.005 % | min. |
Technological properties
Property | ||
---|---|---|
Application areas | Battery components: cans, covers, connector strips | |