Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.29 g/cm³ Show Supplier Material materials with Dichte of 1.29 g/cm³ | ASTM D792 |
Abmessung
Property | Value | Comment |
---|---|---|
Durchmesser | 1.75 mm Show Supplier Material materials with Durchmesser of 1.75 mm | Tolerance +/- 0.02 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 68 MPa Show Supplier Material materials with Biegefestigkeit of 68 MPa | ISO 172 |
Biegemodul | 2.04 GPa Show Supplier Material materials with Biegemodul of 2.04 GPa | ISO 172 |
Dehnung | 29 % Show Supplier Material materials with Dehnung of 29 % | ISO 527-2 |
Elastizitätsmodul | 2.98 GPa Show Supplier Material materials with Elastizitätsmodul of 2.98 GPa | ISO 527-2 |
Härte, Shore A | 76.0 [-] Show Supplier Material materials with Härte, Shore A of 76.0 [-] | ASTM D2240 |
Streckgrenze | 51.0 MPa Show Supplier Material materials with Streckgrenze of 51.0 MPa | ISO 527-2 |
Zugfestigkeit | 20 MPa Show Supplier Material materials with Zugfestigkeit of 20 MPa | ISO 527-2 |
Thermisch
Property | Value | Pressure | Comment |
---|---|---|---|
Glasübergangstemperatur | 80.0 °C Show Supplier Material materials with Glasübergangstemperatur of 80.0 °C | ASTM D3418 | |
Vicat-Erweichungstemperatur | 78.0 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 78.0 °C | ISO 3076 | |
Wärmeformbeständigkeitstemperatur | 68 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 68 °C | 0.45 MPa | ISO 75-2 |
Technological properties
Property | ||
---|---|---|
Application areas | END-USE PARTS: containers, holders - PROTOTYPES: bottles, packaging - ELECTRONICS: covers, cases, products containing diodes - DECORATIONS: lamps, glass-resembling elements - JEWELLERY: rings, necklaces, bracelets | |
Certifications | Food Contact approved | |
Processing methods | Print temperature: 230-250°C, Bed temperature: 90°C |