Abmessung
Property | Value | Comment |
---|---|---|
Durchmesser | 1.75 mm Show Supplier Material materials with Durchmesser of 1.75 mm | Tolerance +/- 0.02 mm |
Mechanisch
Property | Value |
---|---|
Biegefestigkeit | 71 MPa Show Supplier Material materials with Biegefestigkeit of 71 MPa |
Biegemodul | 2.9 GPa Show Supplier Material materials with Biegemodul of 2.9 GPa |
Dehnung | 9 % Show Supplier Material materials with Dehnung of 9 % |
Zugfestigkeit | 45 MPa Show Supplier Material materials with Zugfestigkeit of 45 MPa |
Thermisch
Property | Value |
---|---|
Glasübergangstemperatur | 68.0 °C Show Supplier Material materials with Glasübergangstemperatur of 68.0 °C |
Schmelzpunkt | 176.0 °C Show Supplier Material materials with Schmelzpunkt of 176.0 °C |
Vicat-Erweichungstemperatur | 92.0 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 92.0 °C |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 7.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 7.5 g/10min | 230°C/21.1N |
Technological properties
Property | ||
---|---|---|
Application areas | PROTOTYPES: functional prototypes, small-size models, models with empty spaces - DECORATIONS: complex structures, ornaments with numerous details, vases, jewellery - MECHANISMS: moving elements, mechanisms printed as a whole | |
Processing methods | Print temperature: 190 – 220°C - Bed temperature: 50 – 100°C (when using plates or other means to increase the adhesion, the heating of the bed is not required) - Protect from moisture (Store filament in tightly sealed containers when not in use). |