Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.07 g/cm³ Show Supplier Material materials with Dichte of 1.07 g/cm³ | |
Wasserabsorption | 0.8 % Show Supplier Material materials with Wasserabsorption of 0.8 % | ASTM D570 |
Abmessung
Property | Value | Comment |
---|---|---|
Durchmesser | 1.75 mm Show Supplier Material materials with Durchmesser of 1.75 mm | Tolerance +/- 0.05 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.066 GPa Show Supplier Material materials with Biegemodul of 0.066 GPa | ASTM D790 |
Dehnung | 900 % Show Supplier Material materials with Dehnung of 900 % | ASTM D638 |
Härte, Shore D | 30.0 [-] Show Supplier Material materials with Härte, Shore D of 30.0 [-] | ASTM D2240 |
Rebound Resilience | 72.0 % Show Supplier Material materials with Rebound Resilience of 72.0 % | ASTM D2632 |
Reißfestigkeit | 95.0 kN/m Show Supplier Material materials with Reißfestigkeit of 95.0 kN/m | ASTM D1004 |
Zugfestigkeit | 21.57 MPa Show Supplier Material materials with Zugfestigkeit of 21.57 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 174.0 °C Show Supplier Material materials with Schmelzpunkt of 174.0 °C | ASTM D3418 |
Technological properties
Property | ||
---|---|---|
Application areas | RUBBER ELEMENTS OF MACHINES: Polymer Gaskets, elements that are frequently bent - GADGETS OR THEIR ELEMENTS: phone sleeves and cases, watch-, pulse counter-, pedometer straps - LINKING ELEMENTS: flexible hinges - TOYS OR THEIR ELEMENTS: tires, rubber figures - JEWELLERY: bands, bracelets | |
Processing methods | Print temperature: 200 – 220°C, bed temperature: 50 – 70 °C - to remove the print easier, it is recommended to heat the bed to 110°C |