Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.16 g/cm³ Show Supplier Material materials with Dichte of 1.16 g/cm³ | |
Wasserabsorption | 0.6 % Show Supplier Material materials with Wasserabsorption of 0.6 % | ASTM D570 |
Abmessung
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.066 GPa Show Supplier Material materials with Biegemodul of 0.066 GPa | ASTM D790 |
Dehnung | 680 % Show Supplier Material materials with Dehnung of 680 % | ASTM D638 |
Härte, Shore D | 40.0 [-] Show Supplier Material materials with Härte, Shore D of 40.0 [-] | ASTM D2240 |
Rebound Resilience | 57.0 % Show Supplier Material materials with Rebound Resilience of 57.0 % | ASTM D2632 |
Reißfestigkeit | 115.0 kN/m Show Supplier Material materials with Reißfestigkeit of 115.0 kN/m | ASTM D1004 |
Zugfestigkeit | 26.47 MPa Show Supplier Material materials with Zugfestigkeit of 26.47 MPa | ASTM D638 |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | RUBBER ELEMENTS OF MACHINES: Polymer Gaskets, elements that are frequently bent - GADGETS OR THEIR ELEMENTS: phone sleeves and cases, watch-, pulse counter-, pedometer straps - LINKING ELEMENTS: flexible hinges - TOYS OR THEIR ELEMENTS: tires, rubber figures - JEWELLERY: bands, bracelets | |
Processing methods | Print temperature: 200-220°C, bed temperature: 50-70 °C - printing speed up to 45 mm/s with direct extruder, can be printed with Bowden style extruder at speed 15-30 mm/s - to remove the print easier, it is recommended to heat the bed to 110°C |