Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | ISO 483 |
Abmessung
Property | Value | Comment |
---|---|---|
Durchmesser | 1.75 mm Show Supplier Material materials with Durchmesser of 1.75 mm | Tolerance +/- 0.02 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 1.2 GPa Show Supplier Material materials with Biegemodul of 1.2 GPa | ISO 178 |
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | |
Elastizitätsmodul | 1.4 GPa Show Supplier Material materials with Elastizitätsmodul of 1.4 GPa | ISO 527 |
Zugfestigkeit | 51 MPa Show Supplier Material materials with Zugfestigkeit of 51 MPa | ISO 527 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 180.0 °C Show Supplier Material materials with Schmelzpunkt of 180.0 °C | ISO 1133 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzvolumenflussrate | 180.0 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 180.0 cm³/10min | ISO 11357 |
Technological properties
Property | ||
---|---|---|
Application areas | MECHANICAL PARTS: guides, gears (cog wheels) - TECHNICAL COMPONENTS: slide bearings, nuts | |
Processing methods | Bed temperature: ca. 100°C, Nozzle temperature: 255-270 °C - No drying required |