Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.22 g/cm³ Show Supplier Material materials with Dichte of 1.22 g/cm³ | ASTM D792 |
Abmessung
Property | Value | Comment |
---|---|---|
Durchmesser | 1.75 mm Show Supplier Material materials with Durchmesser of 1.75 mm | Tolerance +/- 0.02 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 73 MPa Show Supplier Material materials with Biegefestigkeit of 73 MPa | ASTM D790 |
Biegemodul | 2.4 GPa Show Supplier Material materials with Biegemodul of 2.4 GPa | ASTM D790 |
Elastizitätsmodul | 2.86 GPa Show Supplier Material materials with Elastizitätsmodul of 2.86 GPa | ASTM D790 |
Zugfestigkeit | 40 MPa Show Supplier Material materials with Zugfestigkeit of 40 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 9 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 9 g/10min | ASTM D1238 , 210°C/2.16Kg |
15 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 15 g/10min | ASTM D1238 , 210°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Application areas | TOYS OR THEIR ELEMENTS: blocks, works or parts thereof, car parts - PROTOTYPES: tools, conceptual models, switching parts, mechanical parts, elements requiring resistance to higher temperatures - SPARE PARTS: elements of machines, devices, vehicles, electronic equipment - TOOLS OR THEIR ELEMENTS: gears, racks, elements requiring high strength - READY PRODUCTS: containers, handles - TOYS OR THEIR ELEMENTS: blocks, robots or their parts, car parts | |
Processing methods | Print temperature 220-245°C, Bed temperature: 50-70°C (when using plates or other means to increase the adhesion, the heating of the bed is not required) |