Allgemein
Property | Value |
---|---|
Partikelgröße D10 | 48.0 - 53.0 μm Show Supplier Material materials with Partikelgröße D10 of 48.0 - 53.0 μm |
Partikelgröße D50 | 60.0 - 66.0 μm Show Supplier Material materials with Partikelgröße D50 of 60.0 - 66.0 μm |
Partikelgröße D90 | 90.0 - 96.0 μm Show Supplier Material materials with Partikelgröße D90 of 90.0 - 96.0 μm |
Schüttdichte | 2.51 - 2.65 g/cm³ Show Supplier Material materials with Schüttdichte of 2.51 - 2.65 g/cm³ |
Rheological Properties
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Andere | 0.4 % Show Supplier Material materials with Andere of 0.4 % | Total Maximum | |
Eisen | 0.2 % Show Supplier Material materials with Eisen of 0.2 % | ||
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | Maximum | |
Sauerstoff | 0.18 % Show Supplier Material materials with Sauerstoff of 0.18 % | ||
Stickstoff | 0.03 % Show Supplier Material materials with Stickstoff of 0.03 % | ||
Titan | Balance | ||
Wasserstoff | 0.015 % Show Supplier Material materials with Wasserstoff of 0.015 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing, Metal Injection Molding, Thermal Spray, Biomedical, Aerospace |