Allgemein
Property | Value |
---|---|
Partikelgröße D10 | 42.0 - 46.0 μm Show Supplier Material materials with Partikelgröße D10 of 42.0 - 46.0 μm |
Partikelgröße D50 | 60.0 - 65.0 μm Show Supplier Material materials with Partikelgröße D50 of 60.0 - 65.0 μm |
Partikelgröße D90 | 85.0 - 90.0 μm Show Supplier Material materials with Partikelgröße D90 of 85.0 - 90.0 μm |
Schüttdichte | 4.65 - 4.8 g/cm³ Show Supplier Material materials with Schüttdichte of 4.65 - 4.8 g/cm³ |
Rheological Properties
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.61 % Show Supplier Material materials with Aluminium of 0.61 % | |
Bor | 0.005 % Show Supplier Material materials with Bor of 0.005 % | Maximum |
Chrom | 17.6 % Show Supplier Material materials with Chrom of 17.6 % | |
Eisen | 18.5 % Show Supplier Material materials with Eisen of 18.5 % | |
Kobalt | 0.17 % Show Supplier Material materials with Kobalt of 0.17 % | |
Kohlenstoff | 0.02 % Show Supplier Material materials with Kohlenstoff of 0.02 % | |
Kupfer | 0.04 % Show Supplier Material materials with Kupfer of 0.04 % | |
Mangan | 0.07 % Show Supplier Material materials with Mangan of 0.07 % | |
Molybdän | 2.89 % Show Supplier Material materials with Molybdän of 2.89 % | |
Nickel | 54.17 % Show Supplier Material materials with Nickel of 54.17 % | |
Niobium | 5.14 % Show Supplier Material materials with Niobium of 5.14 % | |
Phosphor | 0.005 % Show Supplier Material materials with Phosphor of 0.005 % | |
Sauerstoff | 0.01 % Show Supplier Material materials with Sauerstoff of 0.01 % | |
Schwefel | 0.001 % Show Supplier Material materials with Schwefel of 0.001 % | Maximum |
Silizium | 0.07 % Show Supplier Material materials with Silizium of 0.07 % | |
Stickstoff | 0.01 % Show Supplier Material materials with Stickstoff of 0.01 % | |
Titan | 0.97 % Show Supplier Material materials with Titan of 0.97 % | |
Vanadium | 0.04 % Show Supplier Material materials with Vanadium of 0.04 % | |
Wasserstoff | 0.0004 % Show Supplier Material materials with Wasserstoff of 0.0004 % | |
Wolfram | 0.03 % Show Supplier Material materials with Wolfram of 0.03 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing, Metal Injection Molding, Thermal Spray, Biomedical, Aerospace |