Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | ASTM D792 |
Wasserabsorption | 23.0 °C | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | maximum, ASTM D570 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 54.9 MPa Show Supplier Material materials with Biegefestigkeit of 54.9 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 2.16 GPa Show Supplier Material materials with Biegemodul of 2.16 GPa | ASTM D790 |
Dehnung | 23.0 °C | 40 % Show Supplier Material materials with Dehnung of 40 % | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 60 [-] Show Supplier Material materials with Hardness, Rockwell L of 60 [-] | ASTM D785 |
Zugfestigkeit | 23.0 °C | 30.4 MPa Show Supplier Material materials with Zugfestigkeit of 30.4 MPa | ASTM D638 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 85 °C | ASTM D648 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5E-5 - 1E-4 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5E-5 - 1E-4 1/K | ASTM D696 | ||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | UL 746B | |||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | UL 746B | |||
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 107 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 107 °C | ASTM D1525 | |||
Entflammbarkeit | HB UL94 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 4 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | AUDIO/TV/VTR HOUSING, HOUSEHOLD ITEMS |