Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 78.45 MPa Show Supplier Material materials with Biegefestigkeit of 78.45 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 2.75 GPa Show Supplier Material materials with Biegemodul of 2.75 GPa | ASTM D790 |
Dehnung | 23.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 2.22 GPa Show Supplier Material materials with Elastizitätsmodul of 2.22 GPa | ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 110 [-] Show Supplier Material materials with Hardness, Rockwell R of 110 [-] | ASTM D785 |
Streckgrenze | 23.0 °C | 50.99 MPa Show Supplier Material materials with Streckgrenze of 50.99 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 90 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 90 °C | ASTM D648 | |
Heat deflection temperature, 1.80 MPa | 86 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 86 °C | ASTM D648 | |
Relative temperature index, electrical | 60 °C Show Supplier Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |
Relative temperature index, mechanical impact | 60 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |
Relative temperature index, mechanical strength | 60 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |
Vicat-Erweichungstemperatur | 94 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 94 °C | ASTM D1525 | |
Entflammbarkeit | HB UL94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Kriechstromfestigkeit | 23.0 °C | 0 V Show Supplier Material materials with Kriechstromfestigkeit of 0 V | IEC 60112 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 23 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 23 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | ELECTRIC & ELECTRONIC, MISCELLANEOUS GOODS |