Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | maximum, ASTM D570 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 50 MPa Show Supplier Material materials with Biegefestigkeit of 50 MPa | ISO 178 |
Biegemodul | 23.0 °C | 2.03 GPa Show Supplier Material materials with Biegemodul of 2.03 GPa | ISO 178 |
Hardness, Rockwell L | 23.0 °C | 56 [-] Show Supplier Material materials with Hardness, Rockwell L of 56 [-] | ASTM D785 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | ISO 179 |
Zugfestigkeit | 23.0 °C | 28 MPa Show Supplier Material materials with Zugfestigkeit of 28 MPa | ISO 527-1 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 78 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 78 °C | ISO 75 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5E-5 - 1E-4 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5E-5 - 1E-4 1/K | ASTM D696 | ||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | UL 746B | |||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | UL 746B | |||
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | UL 746B | |||
Entflammbarkeit | HB UL94 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 2.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 2.5 g/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | SHEET EXTRUSION & THERMOFORMING, TAPE REEL & BOBBIN, DISPOSABLE CUPS & PLATES & TRAYS |