Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | ASTM D792 |
Wasserabsorption | 23.0 °C | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | maximum, ASTM D570 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 45.1 MPa Show Supplier Material materials with Biegefestigkeit of 45.1 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 1.91 GPa Show Supplier Material materials with Biegemodul of 1.91 GPa | ASTM D790 |
Dehnung | 23.0 °C | 35 % Show Supplier Material materials with Dehnung of 35 % | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 50 [-] Show Supplier Material materials with Hardness, Rockwell L of 50 [-] | ASTM D785 |
Zugfestigkeit | 23.0 °C | 24.52 MPa Show Supplier Material materials with Zugfestigkeit of 24.52 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 8.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 8.5 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | Compounding grades |