Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | ASTM D792 |
Wasserabsorption | 23.0 °C | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | maximum, ASTM D570 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 3.24 GPa Show Supplier Material materials with Biegemodul of 3.24 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 70 [-] Show Supplier Material materials with Hardness, Rockwell L of 70 [-] | ASTM D785 |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 7.5 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 7.5 kJ/m² | ISO 180 |
Streckgrenze | 23.0 °C | 45 MPa Show Supplier Material materials with Streckgrenze of 45 MPa | ASTM D638 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 75 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 75 °C | ASTM D648 | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.1E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.1E-5 1/K | ASTM D696 |
Vicat-Erweichungstemperatur | 91 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 91 °C | ASTM D1525 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 135 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 135 kV/mm | ASTM D149 |
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | IEC 93 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 12 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 12 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | CUTLERY, JEWEL BOX, TOY |