Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 93 MPa Show Supplier Material materials with Biegefestigkeit of 93 MPa | ISO 178 | ||
Biegemodul | 23.0 °C | 2.35 GPa Show Supplier Material materials with Biegemodul of 2.35 GPa | ISO 178 | ||
Dehnung | 23.0 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | ISO 527-2/50 | ||
Elastizitätsmodul | 23.0 °C | 2.4 GPa Show Supplier Material materials with Elastizitätsmodul of 2.4 GPa | ISO 527-2/1 | ||
Elongation at yield | 23.0 °C | 6 % Show Supplier Material materials with Elongation at yield of 6 % | ISO 527-2/50 | ||
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 67 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 67 kJ/m² | ISO 179 | ||
Streckgrenze | 23.0 °C | 61 MPa Show Supplier Material materials with Streckgrenze of 61 MPa | ISO 527-2/50 | ||
Schlagzähigkeit, Charpy ungekerbt | ISO 179, no break |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 139 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 139 °C | ISO 75-2/B | |||
Heat deflection temperature, 1.80 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ISO 75-2/A | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.5E-5 1/K | ISO 11359-2 | ||
Relative temperature index, electrical | 125 °C Show Supplier Material materials with Relative temperature index, electrical of 125 °C | UL 746 | |||
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746 | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL 746 | |||
Vicat-Erweichungstemperatur | 146 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 146 °C | ISO 306/B50 | |||
Entflammbarkeit | HB for 1.9mm and V-2 for 0.4mm UL94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 3 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 3 [-] | IEC 60250 |
Dielektrizitätskonstante, 100 Hz | 23.0 °C | 3.1 [-] Show Supplier Material materials with Dielektrizitätskonstante, 100 Hz of 3.1 [-] | IEC 60250 |
Dissipation factor, 100Hz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 1E-3 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 9E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 9E-3 [-] | IEC 60250 |
Durchschlagfestigkeit | 23.0 °C | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | IEC 60243-1 |
Kriechstromfestigkeit | 23.0 °C | 250 V Show Supplier Material materials with Kriechstromfestigkeit of 250 V | IEC 60112 |
Surface resistivity | 23.0 °C | 1.00E+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+15 Ω/sq | IEC 60093 |
spezifischer Widerstand | 23.0 °C | 1.00E+13 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+13 Ω·m | IEC 60093 |
Optisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 18 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 18 g/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | GENERAL PURPOSE |