Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Dichte of 1.27 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 69 MPa Show Supplier Material materials with Biegefestigkeit of 69 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 2.1 GPa Show Supplier Material materials with Biegemodul of 2.1 GPa | ASTM D790 |
Dehnung | 23.0 °C | 180 % Show Supplier Material materials with Dehnung of 180 % | ASTM D638 |
Elongation at yield | 23.0 °C | 4.5 % Show Supplier Material materials with Elongation at yield of 4.5 % | ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 108 [-] Show Supplier Material materials with Hardness, Rockwell R of 108 [-] | ASTM D785 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 105 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 105 kJ/m² | ASTM D 256 |
Streckgrenze | 23.0 °C | 50 MPa Show Supplier Material materials with Streckgrenze of 50 MPa | ASTM D638 |
Zugfestigkeit | 23.0 °C | 29 MPa Show Supplier Material materials with Zugfestigkeit of 29 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 70 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 70 °C | ASTM D648 | |
Heat deflection temperature, 1.80 MPa | 62 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 62 °C | ASTM D648 | |
Entflammbarkeit | HB for 1.9mm and V-2 for 0.4mm UL94 |
Optisch
Property | Value | Comment |
---|---|---|
Transmission | 90 % Show Supplier Material materials with Transmission of 90 % | ASTM D1003 at 3000 μm |
Technological properties
Property | ||
---|---|---|
Application areas | Sheet, Cosmetic, Construction, Food, Drink, Deco Film |