Property | Value |
---|---|
Dichte | 7.9 g/cm³ Show Supplier Material materials with Dichte of 7.9 g/cm³ |
Mechanisch
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 0.0000166 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.0000166 1/K | 20 to 200°C |
Wärmeleitfähigkeit | 14 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 14 W/(m·K) |
Magnetisch
Property | Value | Comment |
---|---|---|
Relative magnetische Permeabilität | 1.01 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1.01 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 19.5 - 22.0 % Show Supplier Material materials with Chrom of 19.5 - 22.0 % | |
Kohlenstoff | 0.08 Show Supplier Material materials with Kohlenstoff of 0.08 | max. |
Kupfer | 0.25 Show Supplier Material materials with Kupfer of 0.25 | max. |
Mangan | 2.0 - 4.25 % Show Supplier Material materials with Mangan of 2.0 - 4.25 % | |
Molybdän | 2.0 - 3.0 % Show Supplier Material materials with Molybdän of 2.0 - 3.0 % | |
Nickel | 9.0 - 11.0 % Show Supplier Material materials with Nickel of 9.0 - 11.0 % | |
Niobium | 0.25 - 0.8 % Show Supplier Material materials with Niobium of 0.25 - 0.8 % | |
Phosphor | 0.025 Show Supplier Material materials with Phosphor of 0.025 | max. |
Schwefel | 0.01 Show Supplier Material materials with Schwefel of 0.01 | max. |
Silizium | 0.75 Show Supplier Material materials with Silizium of 0.75 | max. |
Stickstoff | 0.25 - 0.5 % Show Supplier Material materials with Stickstoff of 0.25 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | This grade is usually used for high performance surgical implants, like thin bones screws, high mobility hip prosthesis. | |
Cold Forming | This grade has a high ability for cold drawing which means that it is possible to obtain with a wire hard drawn ( dia 8 mm max), a tensile running from 1000 MPa up to 1800 MPa depending on the requirements of the customer. |