Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 48 % Show Supplier Material materials with Dehnung of 48 % | min. |
Flächenreduzierung | 68.0 % Show Supplier Material materials with Flächenreduzierung of 68.0 % | min. |
Zugfestigkeit | 500.0 - 680.0 MPa Show Supplier Material materials with Zugfestigkeit of 500.0 - 680.0 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Other | Available products: Other products: contact the supplier |