Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 32 % Show Supplier Material materials with Dehnung of 32 % | min. |
Flächenreduzierung | 65.0 % Show Supplier Material materials with Flächenreduzierung of 65.0 % | min. |
Zugfestigkeit | 650.0 - 830.0 MPa Show Supplier Material materials with Zugfestigkeit of 650.0 - 830.0 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Other | Available products: Other products: contact the supplier |