Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 25.0 - 40.0 % Show Supplier Material materials with Dehnung of 25.0 - 40.0 % | min., depending on the size |
Zugfestigkeit | 430.0 - 850.0 MPa Show Supplier Material materials with Zugfestigkeit of 430.0 - 850.0 MPa | depending on the size |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 18.0 % Show Supplier Material materials with Chrom of 18.0 % | |
Kohlenstoff | 0.04 Show Supplier Material materials with Kohlenstoff of 0.04 | max. |
Molybdän | 0.4 % Show Supplier Material materials with Molybdän of 0.4 % | |
Nickel | 9.5 % Show Supplier Material materials with Nickel of 9.5 % | |
Schwefel | 3.5 % Show Supplier Material materials with Schwefel of 3.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, chemicals industry, offshore, electronic equipment, food and food processing industry, decoration and household appliances Screw machining: motor shafts, inserts, rivets, screws and nuts, gas couplings, etc. Parts intended for crimping or deforming, etc. Suitable grade for the automotive market: direct injection, common rail, electro-injectors, etc. | |
Corrosion properties | Excellent corrosion resistance in natural environments: waters, rural and urban atmospheres where there are no major acid concentrations, and in food and food processing environments (with reservations in certain special cases: white wines, mustards, etc.) and in certain chemical environments: nitric acid, cold diluted organic acids, etc. Unlike type 1.4301 steels (AISI 304), UGIMA® 4307 can be used in diluted chlorinated environments. Resistant to intergranular corrosion, even after welding. | |
Other | Available products: Other products: contact the supplier |